Our process can begin with many different sources. As platinum accumulate in many places, its recovery can begin from a lot of places and substrates. In fact the first step of our project would change if the basic matter change. Moreover, solutions of phytoremediation provide a lot of substrates and by-products our project could start from. Indeed our process could start from ashes
Sewage Sludge (Incineration) Ashes
The Bioleaching process allow a far better recovery of platinum. Indeed, the drop of pH is required for the metals solubilization. This step could be realized with chemicals as chlorhydric acid in the actual industry. But in order to achieve a greener process as possible, we decided to lower the pH with biological ways, as the leaching accomplished by Thiobacillus. This method is widely use in mines, e.g. for copper mines in South America, so this will be a reliable step already tested in industrial conditions. This method rely on the ability of the bacteria Thiobacilus to acidify its medium until a pH of 1. The bacterium solution is applied on the ashes and liquid part dropping from it constitute the leachate i.e. a very acidified solutions containing solubilized metals particles mostly in ionic form.
This step wouldn't be obligatory in our process, but it could improve our recovery yield while still using a environmentally friendly approach.
This step consist in spreading a Thiobacillus solution on the ashes then recollecting the produced leachate. This step could be also realised not with Thiobacillus but with chemicals solutions.
Once the platinum is leached, we need to recover it. If leaching (by biological or chemical methods) is clearly recommended to improves solubilization of metals, it does not improves the concentrations. As we worked with synthetic biology, we decided to use what it is commonly employed by cells to catch metals, i.e. siderophore. Siderophores are well known to catch iron most of all but some of them have an affinity with others metals as platinum. So in our process, we planned to work with such a siderophore, called Desferrioxamine B. This one is already employed to recover platinum in mines, and have shown high capacity to recover platinum from ores [1].
Recovery yields with DFHOB can reach 75% of the total platinum if both of these conditions are fully respected: a lowering pH level leaching step should be performed, as well as a alcanization of medium (until a pH range between 8 and 9) before addition of siderophore. The last step devoted to rise up the pH level will be realized using a standard buffer, e.g. a Tris buffer.
So where is the innovation in this step? Firstly, in our case, DFHOB won't be applied on the same materials where is commonly used, in our cases not ores but a leachate of ashes. Basically the main difference will be the metal concentration. Secondly, DFHOB is usually synthesized chemically, we'll rather produce it in high amounts with bacteria. Indeed, operon of the Desferrioxamine B biosynthesis will be cloned into a E. coli bacteria strains in order to produce it, hence lowering the costs of required basic matter as production by bacteria needs especially an appropriate medium and good growth conditions. DFHOB is a derivative of diamines moelcule and therefore its Biosynthesis start with a amino acid, lysine. Lysine is quite expansive, and as we are aware about the cost of our process we decided to use a cheap source of lysine the corn steep liquor. Such a lysine source is already in use in industry since it's cheap, amino acid provided, produced in industrial amounts and well known as a excellent source of nitrogen in growth media. So in this step we hope we could produce DFHOB in high quantities with a affordable cost.
Following previous uses of DFHOB, 75% of platinum can be recovered with 3mM DFHOB solution on 100g at 5ppm platinum concentrated ore. That allow us to estimate that in order to reach a 75% yield (max yield obtained) we 'll need to add approximately 3mg of DFHOB per µg of platinum(see Raw calculations).
To sum up, this step consist in adding an appropriated quantity of Siderophore producer E. coli to the leachate.
For instance....; CALCULS POUR 1G COMBIEN PRODUIT UNE ECOLI DE DFHOB,,???
Our engineered E. coli, i.e. our siderophore producer will produce a lot of DFHOB molecules in its cytoplasm after induction. But theory tell us that all produced molecules may not go out of the cell hence the membranous export system of E. coli is not adapted to the DFHOB. To resolve this we decided to realize the lyse of bacteria in order to release the totality of siderophore molecules in the media.
A wide range of industrial lysis technique are available to perform this step. ( MENTON GAULIN ??)
This step consist in lyse the bacterial cells.
Bioleaching : in simple words, leaching is a metal extraction technique which rely on solubilization of metals ores (ore must be soluble and impurities must be insoluble) in a aqueous solution, by using strong acid solutions. The leachate is the solution containing the solubilized metals of interest. Bioleaching in the same process but involves uses of living organism.
DFHOB: Desferioxamine B, is a molecule produced by (among others) Streptomyces pilosus [2] able to catch metals (as platinum) with a very high affinity.
Corn steep liquor: a by-product of an industrial process (wet-milling) applied on corn kernels. As the kernels are steeped in water solution, the process produce an amino acid, vitamins and minerals enriched solution in high volumes.